Cantrolling welding defects

These are the welds with voids ,blow holes or pockets which weaken welds appreciably and gas acts as stress risers from which cracks spread.porosity in welding is a result of dissolved gases or gases released during the welding process ,being trapped in the metal .when there is insufficient time to espace pror to solidification

1 comment:

  1. Excel In Your Exams With Our Expert Test Preparation Services! At Sistem Tutoring, We Offer Tailored Solutions Through Both In-Person Tutoring And Virtual Tutoring Sessions. Our Experienced Tutors Provide Personalized Guidance, Ensuring You Grasp Key Concepts And Ace Your Tests. Choose The Flexibility Of Virtual Tutoring Or The Traditional Approach Of In-Person Sessions For Effective And Comprehensive Test Preparation. Elevate Your Academic Success With Our Dedicated Tutoring Support